Hyundai CCT-D (MS600-66)

Hyundai/Kia CCT-D

Een versnelde corrosietest onder complexe omgevingen moet worden uitgevoerd in overeenstemming met CCT-D van MS600-66

Stap 1: Zout dippen (onderdompeling) @ 50 °C gedurende 2 uur

Stap 2: Bevochtiging @ 50°C / 95%RH gedurende 8 uur

Stap 3: Drogen bij 70°C / 30%RH gedurende 1,5 uur

Stap 4: Drogen @ 70°C / 15%RH gedurende 1,5 uur

Stap 5: Bevochtiging @ 35°C / 100% RH gedurende 6,5 uur

Stap 6: Drogen @ 35°C / 15%RH gedurende 2 uur

Stap 7: Salt Spray @ 35°C / 95%RH gedurende 30 minuten

Stap 8: Invriezen bij -20°C gedurende 20 minuten

Overgangstijden:

Van stap 1 naar stap 2 = 30 minuten

Van stap 2 naar stap 3 = 20 minuten

Van stap 3 naar stap 4 = 20 minuten

Van stap 4 naar stap 5 = 50 minuten

Van stap 5 naar stap 6 = 50 minuten

Van stap 6 naar stap 7 = 20 minuten

Van stap 7 naar stap 8 = 60 minuten

Van stap 8 naar stap 1 = 20 minuten

De hele cyclus is 24 uur en herhaalbaar