Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

Hyundai CCT-D (MS600-66)

Hyundai/Kia CCT-D

Um ensaio acelerado de corrosão em ambiente complexo deve ser efetuado em conformidade com o CCT-D de MS600-66

Passo 1: Mergulho de sal (Imersão) @ 50°C durante 2 horas

Passo 2: Molhar @ 50°C / 95%RH durante 8 horas

Passo 3: Secagem @ 70°C / 30%RH durante 1,5 horas

Passo 4: Secagem @ 70°C / 15%RH durante 1,5 horas

Passo 5: Molhar @ 35°C / 100%RH durante 6,5 horas

Passo 6: Secagem @ 35°C / 15%RH durante 2 horas

Passo 7: Spray de sal @ 35°C / 95%RH por 30 minutos

Passo 8: Congelação @ -20°C por 20 minutos

Tempos de transição:

Do passo 1 para o passo 2 = 30 minutos

Do passo 2 para o passo 3 = 20 minutos

Do passo 3 para o passo 4 = 20 minutos

Do passo 4 para o passo 5 = 50 minutos

Do passo 5 ao passo 6 = 50 minutos

Do passo 6 ao passo 7 = 20 minutos

Do passo 7 ao passo 8 = 60 minutos

Do passo 8 ao passo 1 = 20 minutos

Todo o ciclo é de 24 horas e repetível