The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.
Note: the terms salt spray, salt mist & salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.
Can be used to test the relative resistance to corrosion of metallic coatings, when exposed to an acetic acid salt spray climate at an elevated temperature.
Test specimens are placed in an enclosed chamber and exposed to a continuous indirect spray of acidified (pH 3.1to 3.3) salt water solution, which falls-out on to the specimens at a rate of 1.0 to 2.0ml/80cm²/hour, in a chamber temperature of +35C. This climate is maintained under constant steady state conditions. The test duration is variable.
Chamber volumes of less than 200 Litres are not permitted by this test standard.
This test is also referred to as an ASS test.
For further information on ISO standards visit; www.iso.org
Note; ISO 3769 has been replaced by ISO 9227.