Ascott Analytical . . . Case Study

Customer

Alcoa Fastenings

Subject

Successfully testing for the past 5 years

Key Benefits

Unusually short test is long enough to determine a pass or fail.

Alcoa product undergoing corrosion testing in S450xP Salt Spray Chamber

Alcoa Fastenings, manufacturers of fixings & fasteners, have been successfully testing their products in one of our chambers for the past 5 years.

By comparison to some of the test standards that can be obtained by an Ascott chamber, the duration of the test for this product is unusually only 2 hours long! Which is long enough to determine a pass or fail.

Alcoa have also taken full advantage of having their test chamber serviced regularly and in conjunction with using our recommended Corro-Salt, has ensured their chamber remains in perfect working order.

 

Photograph shows Alcoa product undergoing corrosion testing in S450xP Salt Spray Chamber.