Ascott Kesternich Chamber

KH300 – Fully Automatic, SO2 Gas Dosing Test Chamber  The Kesternich test is a cyclic corrosion test involving condensation humidity and the introduction of sulphur dioxide gas (SO2). A specific volume of SO2 gas, usually 0.2L, 1L or 2L is introduced into the test chamber, the chamber temperature is increased to a predetermined level and […]

ISO 9227 Test Panels

ISO 9227 Test Panels CR4 Grade Steel Corrosion test coupons in accordance with ISO 9227 & VDA 233-102. Ascott CR4 Steel Test panels are used to check the reproducibility and repeatability of the test results for Salt Spray or Cyclic Corrosion Test Chambers, before being used to run ISO 9227 or VDA 233-102. It is […]