Salt spray chamber performance

Temperature range Adjustable from ambient to +50°C/+122°F
Salt spray fall-out rates Adjustable from 0.5 to 2.5 ml per 80 cm2 per hour
Wetting mode (Premium chambers only) Adjustable from ambient to +50°C/+122°F
Drying mode (Premium chambers only) Adjustable from ambient to +50°C/+122°F
 
 

 

    

Standard salt spray chambers   S120is S450is S1000is S2000is
Premium salt spray chambers   S120ip S450ip S1000ip S2000ip
 
Chamber Capacity   120 Ltrs/
4.2cu ft
450 Ltrs/
15.8cu ft
1000 Ltrs/
35.3cu ft
2000 Ltrs/
70.6cu ft
 
Mounting Format   Bench top Floor standing Floor standing Floor standing
 
Loading threshold   280mm/11" 800mm/31.5" 800mm/31.5" 800mm/31.5"
 
Chamber external dims, max W 1315mm/51.8" 1660mm/65.4" 2025mm/80.0" 2885mm/113.6"
  D 680mm/26.8" 840mm/33.1" 1205mm/47.5" 1205mm/47.5"
  H 800mm/31.5" 1510mm/59.5" 1720mm/67.5" 1720mm/67.5"
 
Chamber internal dims, max W 715mm/28.2" 1010mm/39.5" 1300mm/51.2" 2160mm/85.0"
  D 490mm/19.3" 640mm/25.0" 980mm/38.5" 980mm/38.5"
  H 490mm/19.3" 1140mm/45.0" 1320mm/52.0" 1320mm/52.0"
 
Salt solution reservoir ext. dims. W n/a (integral) 460mm/18.1" 560mm/22.0" 560mm/22.0"
  D n/a (integral) 620mm/24.5" 620mm/24.5" 620mm/24.5"
  H n/a (integral) 675mm/26.6" 675mm/26.6" 675mm/26.6"
 
Salt solution reservoir capacity for extra capacity, see optional accessory ACC02   40 Ltrs/
10.5 USgal
80 Ltrs/
21 USgal
115 Ltrs/
30.4 USgal
115 Ltrs/
30.4 USgal
 
Removable slotted sample racks see also optional accessories
ACC17/ACC18)
  4 racks each with 23 angled slots 6 racks each
with 28 angled slots
8 racks each with 46 angled slots 16 racks each with 46 angled slots
 
Chamber construction   Glass reinforced plastic, Polypropylene & PVC parts
 
Color 9 standard colors to choose from
 
Electricity supply
     Standard models
     Premium models


1 phase
1 phase

1 phase
1 phase

1 phase
1 phase

1 phase
3 phase
    Voltage (VAC) and frequency (Hz) dependant on country/region of installation
 
Water   Deionized/distilled for topping up air saturator and making salt solution. Air saturator requires a continuous water connection 0.5-6.0 bar (7.3-87 psi). If air saturator is topped up manually option ACC66 must be ordered
 
Air   Clean dry & oil free, 4.0 to 6.0 bar (58-87psi) with 240 Ltrs (8.5cu.ft) per minute flow
 
Exhaust   3m (10ft) exhaust pipe is provided which should be terminated outside building
 
Drain   3m (10ft) drain pipe provided which should be terminated into floor level drain
 
Operating environment conditions   +15 to +30°C (+59 to 86°F), 85% max RH (non condensing) ambient
 
 
Got to the Ascott On-line Shop
Got to the Ascott Corro-Salt website
Got to the Ascott On-line Shop