CR 1 Test Panels for ASTM B117

Ascott CR1 Steel Test Panels are precision-manufactured reference specimens designed for verifying performance in ASTM B117 Salt Spray Tests and cyclic corrosion testing. These test panels ensure your Salt Spray Chamber or Cyclic Corrosion Test Chamber is compliant, accurate, and reliable.

Why ASTM B117 Test Panels Are Essential

The ASTM B117 salt spray test is one of the most widely used corrosion testing standards. To achieve repeatable and reproducible results, it is vital to check the corrosivity of the chamber using ASTM B117 test panels. During continuous operation, apparatus verification should be carried out every 3 months.

Benefits of the Test Panels

    • Manufactured and tested to ISO 3574
    • Supplied with a Certificate of Conformance and a UKAS Test Certificate
    • Packaged in VCI corrosion-inhibiting paper and vacuum-sealed aluminium wrapping
    • Fully compliant for use in ASTM B117 test procedures

Technical Specifications

    • Material: Cold Rolled Steel CR1
    • Size: 76mm x 127mm (±0.2mm)
    • Thickness: 0.8mm (±0.2mm)
    • Pack Size: 20 panels
    • Product Code: ACC144

Preparation of the Test Panels

    1. Clean panels by degreasing only to remove oil, dirt, or contaminants.
    1. Weigh each panel to the nearest 1.0mg using an analytical balance and record the mass.

Correct Arrangement in the Test Chamber

    • Use a minimum of two test panels.
    • Place panels at a 15°–30° angle from vertical.
    • Position close to the salt fog collection funnels, with spacing at least 100mm from chamber walls.
    • Supports must be inert, such as plastic (optional accessory ACC16 available).

Order Test Panels Today

Keep your corrosion testing accurate and compliant. Ascott CR1 ASTM B117 Test Panels (ACC144) are available now in packs of 20 at Ascottshop.com For more information on ASTM B117 testing, visit the ASTM website.
X

Stay up to date with our e newsletter

Keep up to date with the latest developments about Ascott chambers and the latest updates in test standard specifications by signing up to our e newsletter below.