Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

SFW 2,0 S

Kesternich testing simulates acid rain or industrial chemical exposure  to evaluate the relative corrosion resistance of the coating, substrate, or part itself.  Parts or panels are placed inside a specially designed chamber and are exposed to SO2  and humidity before being evaluated for resistance to corrosion.  SFW 2,0 is a concentration level used in DIN 50018:1997

Find suitable Ascott chambers Click Here