Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

GM4298P

Salt spray/mist testing(General Motors)

This General Motors automotive test standard is based upon test standard ASTM B117. Please see elsewhere in this document for details of ASTM B117.

For further information on General Motors standards visit; www.global.ihs.com