Specifications
| Temperature range | Adjustable from ambient to +50°C/+122°F (Option ACC03 increases temperature range from ambient to +60°C/+140°F) |
| Salt spray fall-out rates | Adjustable from 0.5 to 2 ml per 80 cm2 per hour |
| Wetting mode (Premium chambers only) | Adjustable from ambient to +50°C/+122°F |
| Drying mode (Premium chambers only) | Adjustable from ambient to +50°C/+122°F |
|
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
||
| Standard salt spray chambers | S120iS | S300iS | S450iS | S1000iS | S1300iS | S2000iS | S2600iS | |
| Premium salt spray chambers | S120iP | S300iP | S450iP | S1000iP | S1300iP | S2000iP | S2600iP | |
| Chamber Capacity | 120 Ltrs/ 4.2cu ft |
300 Ltrs/ 10.5 cu ft |
450 Ltrs/ 15.8cu ft |
1000 Ltrs/ 35.3cu ft |
1300 Ltrs/ 49.5cu ft |
2000 Ltrs/ 70.6cu ft |
2600 Ltrs/ 91.8cu ft |
|
| Mounting Format | Bench top | Front Opening Floor Standing | Floor standing | Floor standing | Floor standing | Floor standing | Floor standing | |
| Loading threshold | 280mm/11″ | 1100mm/43.3″ | 800mm/31.5″ | 800mm/31.5″ | 800mm/31.5″ | 800mm/31.5″ | 800mm/31.5″ | |
| Chamber external dims, max | W | 1315mm/51.8″ | 1450mm/57″ | 1660mm/65.4″ | 2025mm/80.0″ | 2025mm/80.0″ | 2885mm/113.6″ | 2885mm/113.6″ |
| D | 680mm/26.8″ | 769mm/30″ | 840mm/33.1″ | 1145mm/45.0″ | 1316mm/51.8″ | 1205mm/47.5″ | 1316mm/51.8″ | |
| H | 800mm/31.5″ | 2010mm/80″ | 1510mm/59.5″ | 1720mm/67.5″ | 1965mm/77.4″ | 1720mm/67.5″ | 1965mm/77.4″ | |
| Chamber internal dims, max | W | 715mm/28.2″ | 855mm/34″ | 1010mm/39.5″ | 1300mm/51.2″ | 1300mm/51.2″ | 2160mm/85.0″ | 2160mm/85.0″ |
| D | 490mm/19.3″ | 601mm/24″ | 640mm/25.0″ | 980mm/38.5″ | 980mm/38.5″ | 980mm/38.5″ | 980mm/38.5″ | |
| H | 490mm/19.3″ | 711mm/27″ reducing to 407mm/16″ | 1140mm/45.0″ | 1320mm/52.0″ | 1500mm/59.0″ | 1320mm/52.0″ | 1500mm/59.0″ | |
| Salt solution reservoir ext. dims. | W | n/a | 560mm/22″ | 425mm/16.0″ Dia | 540mm/21.0″ Dia | 540mm/21.0″ Dia | 540mm/21.0″ Dia | 540mm/21.0″ Dia |
| D | n/a | 620mm/24″ | 425mm/16.0″ Dia | 540mm/21.0″ Dia | 540mm/21.0″ Dia | 540mm/21.0″ Dia | 540mm/21.0″ Dia | |
| H | n/a | 675mm/26″ | 630mm/24.0″ | 635mm/25.0″ | 635mm/25.0″ | 635mm/25.0″ | 635mm/25.0″ | |
| Extra Reservoir capacity? –see optional accessories: ACC59 | ||||||||
| Sample racks? see optional accessories: ACC16,ACC17,ACC18 | ||||||||
| Chamber construction | Glass reinforced plastic, Polypropylene & ABS parts | |||||||
| Color | 9 Standard Colours to choose from | |||||||
| Electricity supply Standard models Premium models |
1 phase 1 phase |
1 phase 1 phase |
1 phase 1 phase |
1 phase 1 phase |
1 phase 1 phase |
1 phase 3 phase |
1 phase 3 phase |
|
| Voltage (VAC) and frequency (Hz) dependent on country/region of installation | ||||||||
| Water Requirements |
Deionized/distilled for topping up air saturator and making salt solution. Air saturator requires a continuous water connection 2.5-5.0 bar (36-73 psi). If air saturator is topped up manually option ACC66 must be ordered. | |||||||
| Air Requirements | Clean dry & oil free, 4.0 to 6.0 bar (58-87psi) with 240 Ltrs (8.5cu.ft) per minute flow | |||||||
| Exhaust Requirements | 3m (10ft) exhaust pipe is provided which should be terminated outside building (See Accessory ACC58) | |||||||
| Drain Requirements | 3m (10ft) drain pipe provided which should be terminated into floor level drain (See Accessory ACC58) | |||||||
| Operating environment conditions | +18 to +23°C (+64 to 73°F), 85% max RH (non condensing) ambient | |||||||