Atmosfär Cyclic Specifications
Atmosfär Cyclic Specifications for range of Corrosion Equipment
| Wetting mode | Temperature range | Adjustable from ambient to +70°C/+158°F |
| Humidity range | Fixed at 95% – 100% RH | |
| Oscillating Salt spray mode | Temperature range | Adjustable from ambient to +60°C/+140°F |
| Salt spray fall-out rates | Adjustable from 5 to 10 Ltrs/m² per hour | |
| Conventional Salt spray mode | Temperature range | Adjustable from ambient to +60°C/+140°F |
| Salt spray fall-out rates | Adjustable from 0.5 to 2 ml per 80 cm² per hour (Option ACC01 increases fallout rate up to 5.5 ml per 80 cm² per hour, Option ACC25 increases fallout rate from 2 – 4 ml per 80 cm² per hour) |
|
| Drying mode | Temperature range | Adjustable from ambient to +70°C/+158°F (Option ACC47/8-13 increases the maximum temperature to 80°C/ 176°F) |
| Humidity range | Uncontrolled | |
| Climatic mode | Temperature/humidity range | See below graph |
Performance Graph |
||
![]() |
Graph showing range of temperature/humidity control for Atmosfär Cyclic Corrosion Testing Equipment.
Contact us for further information or Assistance. |
|

| Atmosfär test chambers
R449A Air Cooled (not available in the EU) CO2 Air Cooled EcoCool (Secondary Cooling Medium) |
Atmosfär Lite
AT1300IP/3 AT1300IP/15 AT1300ip/23 |
Atmosfär -20°C
AT1300IP/1 AT1300IP/13 n/a |
Atmosfär -40°C
AT1300IP/2 AT1300IP/14 n/a |
Atmosfär Lite
AT2600IP/4 AT2600IP/15 AT2600IP/23 |
Atmosfär -20°C
AT2600IP/1 AT2600IP/13 n/a |
Atmosfär -40°C
AT2600IP/2 AT2600IP/14 n/a |
|
| Minimum Controlled Temperature | 20°C/68°F | -20°C/-4°F | -40°C/ -40°F | 20°C/68°F | -20°C/-4°F | -40°C/ -40°F | |
| Chamber Capacity | 1300 Ltrs/45.9 cu.ft | 1300 Ltrs/45.9 cu.ft | 1300 Ltrs/45.9 cu.ft | 2600 Ltrs/91.8 cu.ft | 2600 Ltrs/91.8 cu.ft | 2600 Ltrs/91.8 cu.ft | |
| Chamber weight (estimated, without optional accessories) | 340 kg | 340 kg | 340 kg | 440 kg | 440 kg | 440 kg | |
| Mounting Format | Floor standing | Floor standing | Floor standing | Floor standing | Floor standing | Floor standing | |
| Loading threshold | 800mm/31.5″ | 800mm/31.5″ | 800mm/31.5″ | 800mm/31.5″ | 800mm/31.5″ | 800mm/31.5″ | |
| Chamber external dims, max | W | 2025mm/80.0″ | 2025mm/80.0″ | 2025mm/80.0″ | 2885mm/113.6″ | 2885mm/113.6″ | 2885mm/113.6″ |
| D | 1316mm/51.8″ | 1316mm/51.8″ | 1316mm/51.8″ | 1250mm/49″ | 1250mm/49″ | 1250mm/49″ | |
| H | 1965mm/77.4″ | 1965mm/77.4″ | 1965mm/77.4″ | 1946mm/77.4″ | 1946mm/77.4″ | 1946mm/77.4″ | |
| Chamber internal dims, max | W | 1300mm/51.2″ | 1300mm/51.2″ | 1300mm/51.2″ | 2160mm/85.0″ | 2160mm/85.0″ | 2160mm/85.0″ |
| D | 980mm/38.5″ | 980mm/38.5″ | 980mm/38.5″ | 980mm/38.5″ | 980mm/38.5″ | 980mm/38.5″ | |
| H | 1500mm/59.0″ | 1500mm/59.0″ | 1500mm/59.0″ | 1500mm/59.0″ | 1500mm/59.0″ | 1500mm/59.0″ | |
| Refrigeration unit | W | 650mm/25.6″ | 1125mm/44.3″ | 1125mm/44.3″ | 650mm/25.6″ | 1125mm/44.3″ | 1125mm/44.3″ |
| D | 1350mm/51.8″ | 1354mm/53.3″ | 1354mm/51.8″ | 1350mm/51.8″ | 1354mm/51.8″ | 1354mm/51.8″ | |
| H | 1070mm/42.1″ | 1624mm/63.9″ | 1624mm/63.9″ | 1070mm/42.1″ | 1624mm/63.9″ | 1624mm/63.9″ | |
| Salt solution reservoir | W | 540mm/21″ Dia | 540mm/21″ Dia | 540mm/21″ Dia | 540mm/21″ Dia | 540mm/21″ Dia | 540mm/21″ Dia |
| 90 Ltrs/23 US gal | D | 540mm/21″ Dia | 540mm/21″ Dia | 540mm/21″ Dia | 540mm/21″ Dia | 540mm/21″ Dia | 540mm/21″ Dia |
| Separate unit, one supplied to deliver salt water to the conventional salt spray atomizer | H | 635mm/25″ | 635mm/25″ | 635mm/25″ | 635mm/25″ | 635mm/25″ | 635mm/25″ |
| Salt solution reservoir | W | 840mm/34.0″ | 840mm/34.0″ | 840mm/34.0″ | 840mm/34.0″ | 840mm/34.0″ | 840mm/34.0″ |
| 160 Ltrs/42.2 US gal | D | 500mm/19.7″ | 500mm/19.7″ | 500mm/19.7″ | 500mm/19.7″ | 500mm/19.7″ | 500mm/19.7″ |
| Separate unit, one supplied to deliver salt water to the spray bar | H | 790mm/31.1″ | 790mm/31.1″ | 790mm/31.1″ | 790mm/31.1″ | 790mm/31.1″ | 790mm/31.1″ |
| Chamber construction | Glass reinforced plastic, Polypropylene & ABS parts | ||||||
| Color | 9 standard colours to choose from | ||||||
| Electricity supply | Two 3-phase electrical supplies are required (one for the chamber and one for the separate air conditioning unit). The voltage (VAC) and frequency (Hz) are dependent on country/region of installation (to be confirmed at the time of ordering). | ||||||
| Water | The air saturator, humidity generator and salt solution reservoir all require separate connections to a continuous, pressurized deionized/distilled water supply of 2.5–5.0 bar (36–73 psi). | ||||||
| Air | Clean dry & oil free compressed air, 4.0 to 6.0 bar (58-87psi) with 440 Ltrs (15.5cu.ft) per minute flow. Two separate supplies are required, one for the chamber and one for the separate refrigeration unit | ||||||
| Exhaust | 3m (10ft) exhaust pipe is required which should be terminated outside building (see accessory ACC58) | ||||||
| Drain | 3m (10ft) drain pipe is required which should be terminated into floor level drain (see accessory ACC58) | ||||||
| Operating environment conditions | Indoors, with ambient maintained at +18 to +23°C (+64 to 73°F), 85% max RH (non-condensing). | ||||||