Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

ISO 6270-2 (IC)

Procedure for exposing test specimens in condensation-water atmospheres.

ISO 6270-2 (IC)

This test standard was revised in June 2025, with new method IC added

Test ‘IC’ (Intermittent condensation) – requires changing temperature conditions of 40°C to 25°C, during which humidity changes from condensation level of c.100%RH to control at 50% +/-20%

* The correlation between the above 6270-2 test method and the DIN 50 017 test methods, is:
6270-2 method ‘AHT’ is equivalent to DIN 50 017 method ‘KFW’.