Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

DEF STAN 1053 方法 36

DEF STAN 1053可用于测试涂漆样品在环境温度下暴露于间歇性盐雾气候时的相对耐腐蚀性。

将测试样品放置在封闭的腔室中,并在环境温度下暴露于合成海水溶液的间接喷雾中,该溶液落在样品上。 每天产生雾(盐雾),每次8次,每次10分钟,间隔50分钟,周末不喷洒。

这种 DEF STAN 1053 测试也称为“间歇性”盐雾测试。