日产MES-M0007方法B
日产工程标准 – 复合材料腐蚀试验
NES M-0007用于测量试样暴露于盐雾,干燥和润湿(冷凝水湿度)等腐蚀性条件下时的生锈,起泡和粘附程度
标准方法B需要一个循环腐蚀室,该室可以在盐雾,干燥和润湿之间自动循环。
可以选择以下任何一个周期来运行此测试,以与有关各方达成协议
- CCT-1 – 盐雾(35°C,4小时)→干燥(60°C,2小时)→润湿(50°C,95%相对湿度,2小时)
 - 断续器-2- 盐雾(35°C,2小时)→干燥(60°C,2小时)→润湿(50°C,95%相对湿度,4小时)
 - CCT-4 -盐雾(35°C,10分钟)→干燥(60°C,155分钟)→润湿(60°C,95%相对湿度,75分钟),干燥子程序(60°C,160分钟)→润湿(60°C,95%RH,80分钟)重复5次
 