Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

STD 5711,102

人工大気中での腐食試験 – 塩水噴霧試験

このボルボの自動車試験規格は、ISO 9227(人工大気での塩水噴霧腐食試験)と同じです。ISO 9227規格試験の詳細を見るには 、ここをクリックしてください 。

ボルボ規格の詳細については、こちらをご覧ください。 volvogroup.com/suppliers