BS3900 部件 F9

Kesternich 测试模拟酸雨或工业化学品暴露,以评估涂层、基材或部件本身的相对耐腐蚀性。 零件或面板放置在专门设计的腔室中,并暴露于SO2和湿度下,然后进行耐腐蚀性评估。 以下标准用于此类测试。

BS3900 F9部分用于测试油漆和清漆,并使用连续冷凝确定耐湿性。