D17 1058
中性盐雾试验(雷诺)
可用于测试涂层金属试样在高温下暴露于盐雾气候时的相对耐腐蚀性。
将试样置于封闭的腔室中,并暴露于连续间接喷洒中性(pH 6.5至7.2)盐水溶液,该溶液以1.0至2.0ml / 80cm² /小时的速率在+35C的腔室温度下落到试样上。 这种气候在恒定的稳态条件下保持。 测试持续时间是可变的。
本测试标准不允许腔室容积小于400升。
这是雷诺的测试标准。