BS 7479

人造大气中的盐雾腐蚀测试

可用于测试金属材料的相对耐腐蚀性,有或没有临时或永久的腐蚀保护,当暴露于盐雾气候(中性盐雾或乙酸盐雾或铜加速乙酸盐雾)在高温下。

将试样置于封闭的腔室中,并暴露于中性(pH 6.5至7.2)或酸化(pH3.1至3.3)盐水溶液的连续间接喷雾中,该盐水溶液以1.0至2.0ml / 80cm² /小时的速率在+35C或+50C的腔室温度下落到试样上。 这种气候在恒定的稳态条件下保持。 测试持续时间是可变的。

该标准已被ISO 9227取代。

这些测试也称为NSS,ASS和CASS测试。