ASTM D5894

涂漆金属的环盐雾/紫外线照射

ASTM D5894测试需要两种不同类型的测试设备;符合ASTM G53要求的荧光紫外缩合暴露室和符合ASTM G85附录A5要求的盐雾/干燥室。 有关ASTM G85附录A5的详细信息,请参阅 此处 。