国际标准化组织 ISO 6988 认证

Kesternich 测试模拟酸雨或工业化学品暴露,以评估涂层、基材或部件本身的相对耐腐蚀性。 零件或面板放置在专门设计的腔室中,并暴露于SO2和湿度下,然后进行耐腐蚀性评估。 以下标准用于此类测试。

ISO 6988:1985规定了评估材料或产品对含SO2冷凝水分的抵抗力的方法。 该方法已被发现适用于测试金属和非有机涂层。 提供仪器和材料,测试样品,暴露方法,程序,测试持续时间,样品清洁,结果评估和测试报告。