国际标准化组织 ISO 11503 认证

Kesternich 测试模拟酸雨或工业化学品暴露,以评估涂层、基材或部件本身的相对耐腐蚀性。 零件或面板放置在专门设计的腔室中,并暴露于SO2和湿度下,然后进行耐腐蚀性评估。 以下标准用于此类测试。

ISO 11503测试标准涉及油漆,清漆和相关产品的测试。 指定一种测试方法,用于在标准条件下确定油漆或相关材料的单涂层或多涂层系统在间歇性水冷凝中的阻力。