ISO 6270-2 (AHT)

Procedure for exposing test specimens in condensation-water atmospheres.

This test standard replaces and is similar to DIN 50 017*.

Test ‘AHT’ (condensation atmosphere with alternating humidity & air temperature) – requires changing temperature conditions of 40°C to 18-28°C, during which humidity changes from condensation level of c.100%RH towards ambient humidity level.

* The correlation between the above 6270-2 test method and the DIN 50 017 test methods, is:
6270-2 method ‘AHT’ is equivalent to DIN 50 017 method ‘KFW’.