Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

AA-0224 (AA-P 175)

验证表面涂层和粘合剂粘合的腐蚀行为。

AA-0224 (AA-P 175) 是一项为期 7 天的循环腐蚀测试 (CCT),包括以下步骤:

星期一:根据 AA-0324 开始循环 24 小时盐雾。
周二至周五:根据 AA-0213,08:00 至 16:00 冷凝水恒定气候,温度为 40°C。
从 16:00 到 08:00 在室温下再生(开放室或通风室)周六
至周日:在室温下再生(开放室或通风室)