Ascott salt spray cabinets and chambers – one of the world’s most modern and most versatile salt spray corrosion test systems – and with design, ergonomics and quality that’s in a class of its own. 

Chambers to cover every testing requirement from continuous salt spray test through to condensation humidity and modified tests.

Two specification levels:

Standard

Standard models meet the requirements of basic, continuous salt spray tests conducted at a single temperature only, such as ASTM B117 and similar international test standards, and may be used with pH neutral salt solutions (NSS) or those acidified by the addition of Acetic Acid (ASS) or Cupric Acid (CASS).

Premium

Premium models can perform the same basic salt spray tests, but in addition are equipped with extra features which enable them to undertake ‘modified’ tests such as those defined in ASTM G85. Here conventional salt spray is often combined with one other climate, in a two-part cycle, to accelerate the test. For example: salt spray and condensation humidity (SWAAT) or salt spray and drying (PROHESION) or salt spray and SO2 testing.

Six model sizes:

  • 120 Ltr (4.2 cu ft)
  • 450 Ltr (15.8 cu ft)
  • 1000 Ltr (35.3 cu ft)
  • 1300 Ltr (45.9 cu ft)
  • 2000 Ltr (70.6 cu ft)
  • 2600 Ltr (91.8 cu ft)

All Ascott corrosion test chamber models feature:

  • Low loading threshold for ergonomic loading and unloading.
  • ‘Easy Open’ pneumatically operated canopy, with safety interlock.
  • Dry seal gasket to prevent wetting the operator’s clothes.
  • Timed canopy lock and purge of the cabinet interior with fresh air after testing and before the chamber is opened.
  • Easily accessible salt spray atomizer(s) in transparent hard-wearing acrylic, for ease of maintenance.
  • External portable salt solution tank with wheels, for ease of access to a water source, and an integral drain system for ease of cleaning.
  • Central viewing window for unimpeded visual access to chamber interior and test material.
  • Base castors and integrated fork lift lift truck runners, for ease of transportation.
  • A free choice of canopy colour.
  • Calibration certificate.
  • Consumables spares kit.

Additional features of Premium Salt Spray Chambers:

  • Integrated immersion heater to create condensation humidity, for testing to a wider range of ‘modified’ salt spray tests.
  • Intuitive touch-screen, full color user control interface, employing the latest version of our highly intuitive operating software, for ease of programming and use.
  • The operating software has a very large capacity for the creation of complex multi-step test programmes, so that the widest possible range of test profiles can be accommodated.
  • The icon based control interface offers a variety of languages built-in for ease of understanding and use.
  • RJ45 communications port enabling the chamber to be wired or wirelessly connected to a local area network (LAN) for logging and remote programming via a computer running optional software.
  • A real-time, user configurable ‘clock’ to enable different test samples to be batched and have their exposure time monitored separately, with alarms to warn when a pre-set test period has been completed.