Wetting mode  Temperature range  Adjustable from ambient to +70°C/+158°F
  Humidity range  Fixed at 95% – 100% RH
Oscillating Salt spray mode  Temperature range  Adjustable from ambient to +50°C/+122°F
  Salt spray fall-out rates  Adjustable from 5 to 10 Ltrs/m² per hour
Conventional Salt spray mode  Temperature range  Adjustable from ambient to +50°C/+122°F
  Salt spray fall-out rates  Adjustable from 0.5 to 2.5 ml per 80 cm² per hour
(Option ACC01 increases fallout rate up to 5.5 ml per 80 cm² per hour, Option ACC25 increases fallout rate from 2 – 4 ml per 80 cm² per hour)
Drying mode Temperature range  Adjustable from ambient to +70°C/+158°F
  Humidity range  Uncontrolled
Climatic mode Temperature/humidity range  See adjacent graph

Performance Graph

(click to enlarge)

Graph showing range of temperature/humidity control for Atmosfär chambers

Atmosfär test chambers AT1300iP/Lite AT1300iP/1 AT1300iP/2 AT2600iP/Lite AT2600iP/1 AT2600iP/2
Minimum Controlled Temperature 20°C/68°F -20°C/-4°F -40°C/ -40°F 20°C/68°F -20°C/-4°F -40°C/ -40°F
Chamber Capacity 1300 Ltrs/45.9 cu.ft 1300 Ltrs/45.9 cu.ft 1300 Ltrs/45.9 cu.ft 2600 Ltrs/91.8 cu.ft 2600 Ltrs/91.8 cu.ft 2600 Ltrs/91.8 cu.ft
Chamber weight (estimated, without optional accessories) 340 kg 340 kg 340 kg 440 kg 440 kg 440 kg
Mounting Format Floor standing Floor standing Floor standing Floor standing Floor standing Floor standing
Loading threshold 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″
Chamber external dims, max W 2025mm/80.0″ 2025mm/80.0″ 2025mm/80.0″ 2885mm/113.6″ 2885mm/113.6″ 2885mm/113.6″
D 1316mm/51.8″ 1316mm/51.8″ 1316mm/51.8″ 1316mm/51.8″ 1316mm/51.8″ 1316mm/51.8″
H 1965mm/77.4″ 1965mm/77.4″ 1965mm/77.4″ 1965mm/77.4″ 1965mm/77.4″ 1965mm/77.4″
Chamber internal dims, max W 1300mm/51.2″ 1300mm/51.2″ 1300mm/51.2″ 2160mm/85.0″ 2160mm/85.0″ 2160mm/85.0″
D 980mm/38.5″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″
H 1500mm/59.0″ 1500mm/59.0″ 1500mm/59.0″ 1500mm/59.0″ 1500mm/59.0″ 1500mm/59.0″
Refrigeration unit W 1510mm/59.4″ 1510mm/59.4″ 1510mm/59.4″ 1510mm/59.4″ 1510mm/59.4″ 1510mm/59.4″
D 1550mm/60.0″ 1550mm/60.0″ 1550mm/60.0″ 1550mm/60.0″ 1550mm/60.0″ 1550mm/60.0″
H 1055mm/41.5″ 1055mm/41.5″ 1055mm/41.5″ 1055mm/41.5″ 1055mm/41.5″ 1055mm/41.5″
Salt solution reservoir W 560mm/22.0″ 560mm/22.0″ 560mm/22.0″ 560mm/22.0″ 560mm/22.0″ 560mm/22.0″
115 Ltrs/30.4 US gal D 620mm/24.5″ 620mm/24.5″ 620mm/24.5″ 620mm/24.5″ 620mm/24.5″ 620mm/24.5″
Separate unit, one supplied to deliver salt water to the conventional salt spray atomizer H 675mm/26.6″ 675mm/26.6″ 675mm/26.6″ 675mm/26.6″ 675mm/26.6″ 675mm/26.6″
Salt solution reservoir W 840mm/34.0″ 840mm/34.0″ 840mm/34.0″ 840mm/34.0″ 840mm/34.0″ 840mm/34.0″
160 Ltrs/42.2 US gal D 500mm/19.7″ 500mm/19.7″ 500mm/19.7″ 500mm/19.7″ 500mm/19.7″ 500mm/19.7″
Separate unit, one supplied to deliver salt water to the spray bar H 790mm/31.1″ 790mm/31.1″ 790mm/31.1″ 790mm/31.1″ 790mm/31.1″ 790mm/31.1″
Chamber construction Glass reinforced plastic, Polypropylene & PVC parts
Color 9 standard colors to choose from
Electricity supply Two 3-phase electrical supplies are required (one for the chamber and one for the separate air conditioning unit). The voltage (VAC) and frequency (Hz) are dependent on country/region of installation (to be confirmed at the time of ordering).
Water The air saturator, humidity generator and salt solution reservoir all require separate connections to a continuous, pressurized deionized/distilled water supply of 2.0–5.0 bar (29–73 psi).
Air Clean dry & oil free compressed air, 4.0 to 6.0 bar (58-87psi) with 240 Ltrs (8.5cu.ft) per minute flow. Two separate supplies are required, one for the chamber and one for the separate salt solution reservoir.
Exhaust 3m (10ft) exhaust pipe is provided which should be terminated outside building.
Drain 3m (10ft) drain pipe provided which should be terminated into floor level drain.
Operating environment conditions Indoors, with ambient maintained at +18 to +23°C (+64 to 73°F), 85% max RH (non-condensing).