Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist & salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

STD 5711,102

Corrosion Test in artificial atmospheres – salt spray tests

This Volvo automotive test standard is the same as ISO 9227 (Salt spray corrosion tests in artificial atmospheres). Click here to view details of the ISO 9227 standard test.