D17 1058

Neutral salt spray test (Renault)

Can be used to test the relative resistance to corrosion of coated metallic specimens, when exposed to a salt spray climate at an elevated temperature.

Test specimens are placed in an enclosed chamber and exposed to a continuous indirect spray of neutral (pH 6.5 to 7.2) salt water solution, which falls-out on to the specimens at a rate of 1.0 to 2.0ml/80cm²/hour, in a chamber temperature of +35C. This climate is maintained under constant steady state conditions. The test duration is variable.

Chamber volumes of less than 400 Litres are not permitted by this test standard.

This is a Renault test standard.