Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist & salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

BS2011 Part2.1 Ka

Basic environmental testing procedures, salt mist

Can be used to test the relative resistance to corrosion of protective coatings, when exposed to a salt mist (spray) climate at an elevated temperature.

Test specimens are placed in an enclosed chamber and exposed to a continuous indirect spray of neutral (pH 6.5 to 7.2) salt water solution, which falls-out on to the specimens at a rate of 1.0 to 2.0ml/80cm²/hour, in a chamber temperature of +35C. This climate is maintained under constant steady state conditions. The test duration is variable.

This test is also referred to as a Neutral Salt Spray or NSS test.

For further information on British standards visit; www.bsigroup.com

Note; BS2011 Part2.1 Kb has been replaced by BS EN 60068-2-11.

Find suitable Ascott chambers Click Here