AA-0213 (AA-P 224)

Condensation Water Constant Atmosphere Test

This test serves to evaluate the resistance of automotive coatings and painted hang-on parts to high humidity. Test specimens are placed in an enclosed chamber and exposed to constant conditions of +40°C and constant condensation humidity level of c.100% RH.

In all other respects this test is based upon DIN EN ISO 6270-2 KK.