DEF STAN 00-35 Part 3 test CN2

Salt (corrosive) atmospheres

The purpose of this defence standard test is to determine the resistance of material to salt laden atmospheres. It covers two different test methods, which are referred to at the ‘salt mist test’ and the ‘salt corrosion test’. Details as follows:

Salt mist test

This test is based upon test standard BS EN 60068-2-11. Please see elsewhere in this document for details of BS EN 60068-2-11.

Salt corrosion test

This test is based upon test standard BS EN 60068-2-52. Please see elsewhere in this document for details of BS EN 60068-2-52.