The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.
Note: the terms salt spray, salt mist & salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.
This standard specifies the preparation of 3 ‘stock’ solutions containing inorganic salts in proportions and concentrations representative of ocean water.
For further information on ASTM standards visit; www.astm.com