Print

Standard Corrosion Tests

Click on Test Standard Number to show more detail

Test Standard
Number
Country/ 
Industry/
Company
of Origin
Standard
Salt Spray
Chambers
Premium
Salt Spray
Chambers
CCT
Chambers
Atmosfär
Chambers
Required Optional Accessories

ACC plus suffix below
S120iS
S450iS
S1000iS
S1300iS
S2000iS
S2600iS
S120iP
S450iP
S1000iP
S1300iP
S2000iP
S2600iP
CC450iP
CC1000iP
CC1300iP
CC2000iP
CC2600iP
AT1300iP/1
AT1300iP/2
AT26000iP/1
AT2600iP/2
01
25
29
30
32
34
42
46
112
86
Condensation Humidity Test Standards
  AA-0213
  (AA-P 224)
 BMW                      
  AA-0224
  (AA-P 175)
 BMW                        
  ASTM D2247  USA  
not 120 Ltr chamber
                   
  BS 3900 Part F2  UK                           
  DIN 50 017-KK  Germany                      
  DIN 50 017-KFW  Germany                      
  DIN 50 017-KTW  Germany                      
  ISO 6270-2 (AHT)  Europe                      
  ISO 6270-2 (AT)  Europe                      
  ISO 6270-2 (CH)  Europe                      
  VDA 621-421  Germany                      
Water Fog Humidity Test Standards
  ASTM D1735  USA         •*          
  GM4465P  General
 Motors
        •*          
Salt Spray/Mist/Fog Test Standards
  50180 method A1  Fiat                    
  50180 method A2  Fiat                    
  50180 method A3  Fiat                    
  AA-0324
  (AA-P 184)
 BMW                    
  AS 2331 meth.3.1  Australia
not 120 Ltr chamber

not 120 Ltr chamber
                   
  AS 2331 meth.3.2  Australia
not 120 Ltr chamber

not 120 Ltr chamber
                   
  AS 2331 meth.3.3  Australia
not 120 Ltr chamber

not 120 Ltr chamber
                   
  ASTM B117  USA                    
  ASTM B287  USA                    
  ASTM B368  USA                    
  ASTM G43  USA                      
  ASTM G85
  annex A1
 USA                    
  ASTM G85
  annex A2
 USA                      
  ASTM G85
  annex A3
 USA                      
  ASTM G85
  annex A4
 USA                    
  ASTM G85
  annex A5
 USA                      
  ASTM G5894  USA                      
  BS2011 Part2.1 Ka  UK                    
  BS2011 Part2.1 Kb  UK                    
  BS 3900 Part F4  UK                    
  BS 3900 Part F12  UK
not 120 Ltr chamber

not 120 Ltr chamber
                   
  BS 5466 Part 1  UK
not 120 Ltr chamber

not 120 Ltr chamber
                   
  BS 5466 Part 2  UK
not 120 Ltr chamber

not 120 Ltr chamber
                   
  BS 5466 Part 3  UK
not 120 Ltr chamber

not 120 Ltr chamber
                   
  BS 7479  UK
not 120 Ltr chamber

not 120 Ltr chamber
                   
  D17 1058  Renault
not 120 Ltr chamber

not 120 Ltr chamber
                  
  DEF STAN 00-35
  Pt3 CN2
 UK
 Defence
                  
  DEF STAN 133
  method 14
 UK
 Defence
                  
  DEF STAN 1053
  method 24
 UK
 Defence
                  
  DEF STAN 1053
  method 36
 UK
 Defence
                    
  DIN 50 021-SS  Germany                   
  DIN 50 021-ESS  Germany                   
  DIN 50 021-CASS  Germany                   
  EN 60068-2-11  Europe                    
  EN 60068-2-52  Europe                
  EN 60512-11-6  Europe                   
  EN ISO 4541  Europe                        
  EN ISO 7253  Europe
not 120 Ltr chamber

not 120 Ltr chamber
                   
  FLTM BI 103-01  Ford                   
  GM4298P  General
 Motors
                  
  IEC 68-2-11  Europe                   
  IEC 68-2-52  Europe                   
  IEC 60068-2-11  Europe                   
  IEC 60068-2-52  Europe                
  ISO 3768  Europe
not 120 Ltr chamber

not 120 Ltr chamber
                  
  ISO 3769  Europe
not 120 Ltr chamber

not 120 Ltr chamber
                  
  ISO 3770  Europe
not 120 Ltr chamber

not 120 Ltr chamber
                  
  ISO 7253  Europe
not 120 Ltr chamber

not 120 Ltr chamber
                  
  ISO 9227  Europe                   
  JIS H 8502 M1  Japan
not 120 Ltr chamber

not 120 Ltr chamber
                  
  JIS H 8502 M2  Japan
not 120 Ltr chamber

not 120 Ltr chamber
                  
  JIS H 8502 M3  Japan
not 120 Ltr chamber

not 120 Ltr chamber
                  
  JIS Z 2371  Japan
not 120 Ltr chamber

not 120 Ltr chamber
                  
  JNS 30.16.03  Jaguar                   
  MIL-STD-202  USA
 Military
                  
  MIL-STD-750
  method 1046
 USA
 Military
                  
  MIL-STD-810G  USA
 Military
                
  NFX 41-002  France                   
  RTCA/DO-160  RTCA Inc.                   
  STD 5711,102  Volvo                   
  TPJLR.52.252  Jaguar 
Land Rover
                  
  VG 95 210  Germany                   
Cyclic Corrosion Test (CCT) Standards
  AS 2331
  M 3.13 Cycle A
 Australia                       
  AS 2331
  M 3.13 Cycle B
 Australia                       
  AS 2331
  M 3.13 Cycle C
 Australia                       
  AS 2331
  M 3.13 Cycle E
 Australia                         
  ASTM G44  USA                       
  CCT-1  Japan
 Automotive
                   
  CCT-2  Japan
 Automotive
                   
  CCT-4  Japan
 Automotive
                   
  CETP00.00-L-467  Ford                          
  ECC-1  Renault                      
  D17 2028  Renault                      
  GM9540P  General
 Motors
        •*        
  GMW14872  General
 Motors
        •*        
  ISO11997-Cycle A  Europe                    
  ISO11997-Cycle B  Europe                    
  ISO14993  Europe                    
  ISO 16701  Europe                          
  JASO M 609  Japan
 Automotive
                   
  JASO M 610  Japan
 Automotive
                   
  JIS H 8502 M4  Japan                        
  JIS H 8502 M5  Japan                      
  P-VW 1209  VW/Audi                           
  P-VW 1210  VW/Audi                    
  SAE J 2334  USA
 Automotive
           o* o        
  STD 423-0014  Volvo                          
  STD 4233  Volvo                          
  STD 4319  Scania                          
  STD 4445  Scania                          
  STD1027, 14  Volvo                          
  STD1027,1375  Volvo                          
  TSH1555G  Toyota                        
  VCS 1027,149  Volvo                          
  VCS 1027,1449  Volvo                          
  VDA 233-102  Germany
 Automotive
                   
  VDA 621-415  Germany
 Automotive
                   
Miscellaneous Test Standards
  DIN 50 014  Germany                    
  ASTM D1748  USA