Print

Salt Spray Chamber Chamber Accessories

Data Measurement & Recording

All Ascott test chambers are supplied complete and ready to run. The following optional accessories may not therefore be necessary, but some may be considered desirable. Use the menu above to select other chamber accessory sections.

F = factory fitted only  A = available separately

 

Optional accessory

Reference   

Description

F/A

 

1 pen chart recorder paper type

ACC08/1

1 pen, 100mm/4” wide, paper strip chart recorder, coupled to a temperature sensor, for continuously recording the chamber air temperature (°C).

F

 

2 pen chart recorder paper type

ACC08/2

ONLY AVAILABLE FOR PREMIUM SALT SPRAY CHAMBERS

2 pen, 100mm/4” wide, paper strip chart recorder, coupled to temperature and humidity sensors, for continuously recording the air temperature (°C) and relative humidity (%RH).

F

 

Hand held pH meter

ACC11

Digital pH meter, for measuring the pH of salt solution fallout over range 0-14 pH with a resolution of 0.01 pH. Supplied complete with buffers.

A

 

Hand held temperature & humidity probe

Hand held temperature & humidity probe

ACC28

Precision hand-held thermo-hygrometer for independently checking the chamber temperature and humidity. Includes a special salt resistant measuring probe mounted on an extension cable. Range: -40 to +85°C & 0 to 100%RH. Requires any size entry port (see option ACC10) to access the chamber interior.

A

 

Re-transmission of temperature & humidity

ACC36

ONLY AVAILABLE FOR PREMIUM SALT SPRAY CHAMBERS

Re-transmission of chamber temp & humidity as 2 x 0-10VDC signals via externally mounted socket. For remote data logging.

F

 

Thermometer pocket in air saturator

ACC37

This option provides a 6mm/0.24” internal diameter thermopocket, mounted in the air saturator. Users may insert their own independent temperature probe into this, if they wish to independently monitor the air saturator temperature.

F

 

2 pen chart recorder - paperless type ††

2 pen chart recorder - paperless

ACC40/2

ONLY AVAILABLE FOR PREMIUM SALT SPRAY CHAMBERS

2 pen paperless chart recorder, coupled to temperature and humidity sensors, for continuously recording the chamber air temperature (°C) and relative humidity (%RH). Records values electronically on to a virtual chart. Data can be stored on integral USB drive and/or downloaded to a network computer running appropriate software (see option ACC41) via RJ45 (Ethernet) connector.

†† Recorder is free-standing for 120 Ltrs chambers, & chamber mounted for other models.

F

 

Software for paperless chart recorder ACC40/2

ACC41

ONLY AVAILABLE FOR PREMIUM SALT SPRAY CHAMBERS

Software for paperless chart recorder (separate option ACC40/2). When loaded on a network computer enables monitoring and graphical storage of actual chamber temperature and humidity profiles.

For accessory ACC40/2

A

 

Temperature data logger

ACC50

A battery powered, chamber mounted data logger and temperature sensor. Continuously records the chamber air temperature (°C). Logs can be downloaded to a computer running appropriate software (provided).

F

 

Temperature & humidity data logger

ACC52

As ACC50, but also records humidity (%RH) levels using a combined temperature and humidity sensor. Requires any size entry port (see option ACC10) to access the chamber interior.

F

 

Salt solution reservoir low level alarm

ACC70

Operates if the salt solution level falls below requirement for approximately 18 hours testing low level alarm at 1-2ml/hour fall-out rates. Sounds audible alarm and displays warning message. If reservoir is not refilled within 18 hours the running chamber program will automatically pause/stop.

F

 

Hand-held salinity refractometer

Hand-held salinity refractometer

ACC100

A salinity refractometer optimized to give a direct reading of percentage sodium chloride in the range 0 to 28%, with automatic temperature compensation. A single drop of the salt solution to be measured is placed on the viewing window, using the pipette supplied, and its salinity read against a high contrast scale, graduated in % sodium chloride, to give an accurate reading.

A

 

Salt solution consumption sensor

ACC102

ONLY AVAILABLE FOR PREMIUM SALT SPRAY CHAMBERS

This option comprises of an electronic liquid flow sensor mounted inside the chamber and sensor situated in-line between the salt solution reservoir and the salt spray atomizer. The sensor measures the flow of salt solution from the reservoir to the atomizer. The output from the is displayed digitally at the chamber HMI as instantaneous consumption in ml per min and total consumption in ml.

F

 

Temperature & humidity sensor extension cable

ACC104

ONLY AVAILABLE FOR PREMIUM SALT SPRAY CHAMBERS

Extension cable to allow chamber sensor to be positioned (& chamber to be controlled) at any point inside chamber.

A

 

Fallout measuring kit

Fallout measuring kit

ACC108

Comprises of 4 x 100ml measuring cylinders and 4 x 100mm funnels, for manually collecting and measuring salt spray fall-out inside a chamber, during salt spray testing.

A

 

Software for suffix iP chambers

Software for suffix iP chambers

ACC120

ONLY AVAILABLE FOR PREMIUM SALT SPRAY CHAMBERS

This software allows logging of chamber variables and editing of chamber programs. It is uses a graphics based display which mimics and improves on the chamber interface.

It can be loaded on Workstations or Laptops with Operating systems of Windows 8 Professional, Windows 7 Professional, Windows 2000 (SP4+), Windows XP Professional (SP3+). It also requires the following minimum hardware requirements - 1 GHz Processor minimum Processor, 256 MB RAM, video 1280 x 1024 (high colour 16 bit) and it is advised 2GB Hard Disk Space for data. The software communicates via an Ethernet network adaptor from chamber to PC / Laptop. The Workstation / Laptop also require a USB port to load the software and to accommodate the Dongle that is needed to run this software.

Network must also be suitable as it will only work across a network on Class C subnet masks/ IP addresses – please liaise with your IT departments to confirm this or contact Ascott for further information.

A

 

Software for suffix iP chambers

Software for suffix iP chambers

ACC121

ONLY AVAILABLE FOR PREMIUM SALT SPRAY CHAMBERS

This software allows logging of chamber variables and editing of chamber programs. It is uses a graphics based display which mimics and improves on the chamber interface.

It can be loaded on Workstations or Laptops with Operating systems of Windows 8 Professional, Windows 7 Professional, Windows 2000 (SP4+), Windows XP Professional (SP3+). It also requires the following minimum hardware requirements - 1 GHz Processor minimum Processor, 256 MB RAM, video 1280 x 1024 (high colour 16 bit) and it is advised 2GB Hard Disk Space for data. The software communicates via an Ethernet network adaptor from chamber to PC / Laptop. The Workstation / Laptop also require a USB port to load the software and to accommodate the Dongle that is needed to run this software.

This version of the logging software improves on the ACC120 version by the introduction of a router inside the chamber that allows it to work across a networks on Class A & B subnet masks/ IP addresses. The Workstation / Laptop on the network must be set to an advised static IP address to communicate – dynamic addressing will not work – please liaise with your IT departments to confirm that this is possible before purchasing the software.

A

 

Software ACC120 pre-installed on Laptop Computer

Software ACC120

ACC122

ONLY AVAILABLE FOR PREMIUM SALT SPRAY CHAMBERS

This option comprises of the ACC120 software pre-installed on a laptop computer. A wireless router is also included for the chamber, to enable the computer and chamber to communicate wirelessly, if required. Everything is configured and ready to run.

A

 

Real-time monitoring of chamber control variables (iPad Application)

Software ACC120

ACC124

This option comprises of an iPad application for wireless monitoring of chamber variables such as temperature, humidity and salt fog fall-out rate. Only available for chambers equipped with Electronic Catchpots - optional accessory ACC116. Both the iPad and the chamber need to be connected to the same Local Area Network (LAN). iPad not supplied.

A