Specifications

Temperature range Adjustable from ambient to +50°C/+122°F
(Option ACC03 increases temperature range from ambient to +60°C/+140°F)
Salt spray fall-out rates Adjustable from 0.5 to 2.5 ml per 80 cm2 per hour
Wetting mode (Premium chambers only) Adjustable from ambient to +50°C/+122°F
Drying mode (Premium chambers only) Adjustable from ambient to +50°C/+122°F

    

Standard salt spray chambers S120is S450is S1000is S1300is S2000is S2600is
Premium salt spray chambers S120ip S450ip S1000ip S1300ip S2000ip S2600ip
Chamber Capacity 120 Ltrs/
4.2cu ft
450 Ltrs/
15.8cu ft
1000 Ltrs/
35.3cu ft
1300 Ltrs/
49.5cu ft
2000 Ltrs/
70.6cu ft
2600 Ltrs/
91.8cu ft
Mounting Format Bench top Floor standing Floor standing Floor standing Floor standing Floor standing
Loading threshold 280mm/11″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″
Chamber external dims, max W 1315mm/51.8″ 1660mm/65.4″ 2025mm/80.0″ 2025mm/80.0″ 2885mm/113.6″ 2885mm/113.6″
D 680mm/26.8″ 840mm/33.1″ 1205mm/47.5″ 1316mm/51.8″ 1205mm/47.5″ 1316mm/51.8″
H 800mm/31.5″ 1510mm/59.5″ 1720mm/67.5″ 1965mm/77.4″ 1720mm/67.5″ 1965mm/77.4″
Chamber internal dims, max W 715mm/28.2″ 1010mm/39.5″ 1300mm/51.2″ 1300mm/51.2″ 2160mm/85.0″ 2160mm/85.0″
D 490mm/19.3″ 640mm/25.0″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″
H 490mm/19.3″ 1140mm/45.0″ 1320mm/52.0″ 1500mm/59.0″ 1320mm/52.0″ 1500mm/59.0″
Salt solution reservoir ext. dims. W n/a (integral) 460mm/18.1″ 560mm/22.0″ 560mm/22.0″ 560mm/22.0″ 560mm/22.0″
D n/a (integral) 620mm/24.5″ 620mm/24.5″ 620mm/24.5″ 620mm/24.5″ 620mm/24.5″
H n/a (integral) 675mm/26.6″ 675mm/26.6″ 675mm/26.6″ 675mm/26.6″ 675mm/26.6″
Salt solution reservoir capacity for extra capacity, see optional accessory ACC02 40 Ltrs/
10.5 USgal
80 Ltrs/
21 USgal
115 Ltrs/
30.4 USgal
115 Ltrs/
30.4 USgal
115 Ltrs/
30.4 USgal
115 Ltrs/
30.4 USgal
Removable slotted sample racks see also optional accessories
ACC17/ACC18)
4 racks each with 23 angled slots 6 racks each
with 28 angled slots
8 racks each with 46 angled slots 8 racks each with 46 angled slots 16 racks each with 46 angled slots 16 racks each with 46 angled slots
Chamber construction Glass reinforced plastic, Polypropylene & PVC parts
Color 9 standard colors to choose from
Electricity supply
Standard models
Premium models
1 phase
1 phase
1 phase
1 phase
1 phase
1 phase
1 phase
1 phase
1 phase
3 phase
1 phase
3 phase
Voltage (VAC) and frequency (Hz) dependant on country/region of installation
Water Deionized/distilled for topping up air saturator and making salt solution. Air saturator requires a continuous water connection 2.0-5.0 bar (29-72 psi). If air saturator is topped up manually option ACC66 must be ordered.
Air Clean dry & oil free, 4.0 to 6.0 bar (58-87psi) with 240 Ltrs (8.5cu.ft) per minute flow
Exhaust 3m (10ft) exhaust pipe is provided which should be terminated outside building
Drain 3m (10ft) drain pipe provided which should be terminated into floor level drain
Operating environment conditions +18 to +23°C (+64 to 73°F), 85% max RH (non condensing) ambient