Specifications

Wetting mode  Temperature range  Adjustable from ambient to +70°C/+158°F
  Humidity range  Fixed at 95% – 100% RH
Salt spray mode  Temperature range  Adjustable from ambient to +50°C/+122°F
  Salt spray fall-out rates  Adjustable from 0.5 to 2.5 ml per 80 cm² per hour
(Option ACC01 increases fallout rate up to 5.5 ml per 80 cm² per hour, Option ACC25 increases fallout rate from 2 – 4 ml per 80 cm² per hour)
Drying mode Temperature range  Adjustable from ambient to +70°C/+158°F
  Humidity range  Uncontrolled
Controlled humidity mode Temperature/humidity range  See graph

Performance Graph

(click to enlarge)

Graph showing standard range of temperature/humidity control for a CCT chamber and how this may be extended by the addition of optional accessories.
Cyclic corrosion test chambers CC450ip CC1000ip CC1300ip CC2000ip CC2600ip
Chamber Capacity 450 Ltrs/
15.8cu ft
1000 Ltrs/
35.3cu ft
1300 Ltrs/
45.9cu ft
2000 Ltrs/
70.6cu ft
2600 Ltrs/
91.8cu ft
Mounting Format Floor standing Floor standing Floor standing Floor standing Floor standing
Loading threshold 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″
Chamber external dims, max W 1660mm/65.4″ 2025mm/80.0″ 2025mm/80.0″ 2885mm/113.6″ 2885mm/113.6″
D 840mm/33.1″ 1205mm/47.5″ 1316mm/51.8″ 1205mm/47.5″ 1316mm/51.8″
H 1510mm/59.5″ 1720mm/67.5″ 1965mm/77.4″ 1720mm/67.5″ 1965mm/77.4″
Chamber internal dims, max W 1010mm/39.5″ 1350mm/51.0″ 1300mm/51.2″ 2160mm/85.0″ 2160mm/85.0″
D 640mm/25.0″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″
H 1140mm/45.0″ 1320mm/52.0″ 1500mm/59.0″ 1320mm/52.0″ 1500mm/59.0″
Salt solution reservoir ext. dims. W 460mm/18.1″ 560mm/22.0″ 560mm/22.0″ 560mm/22.0″ 560mm/22.0″
D 620mm/24.5″ 620mm/24.5″ 620mm/24.5″ 620mm/24.5″ 620mm/24.5″
H 675mm/26.6″ 675mm/26.6″ 675mm/26.6″ 675mm/26.6″ 675mm/26.6″
Salt solution reservoir capacity for extra capacity, see optional accessory ACC02 80 Ltrs/
21 USgal
115 Ltrs/
30.4 USgal
115 Ltrs/
30.5 USgal
115 Ltrs/
30.5 USgal
115 Ltrs/
30.5 USgal
Removable slotted sample racks see also optional accessories
ACC17/ACC18)
6 racks each
with 28 angled slots
8 racks each with 46 angled slots 8 racks each with 46 angled slots 16 racks each with 46 angled slots 16 racks each with 46 angled slots
Chamber construction Glass reinforced plastic, Polypropylene & PVC parts
Color 9 standard colours to choose from
Temperature range Adjustable from ambient to +50°C/+122°F
Salt spray fall-out rates Adjustable from 0.5 to 2.5 ml per 80 cm² per hour
Electricity supply 3 phase 3 phase 3 phase 3 phase 3 phase
Voltage (VAC) and frequency (Hz) dependant on country/region of installation
Water Deionized/distilled for topping up air saturator and making salt solution. Air saturator requires a continuous water connection 2.0-5.0 bar (29-72 psi). If ACC42 is ordered the continuous water supply must be pressuried 4.0 – 5.0 bar (58-72 psi). If air saturator is topped up manually option ACC66 must be ordered.
Air Clean dry & oil free, 4.0 to 6.0 bar (58-87psi) with 240 Ltrs (8.5cu.ft) per minute flow
Exhaust 3m (10ft) exhaust pipe is provided which should be terminated outside building
Drain 3m (10ft) drain pipe provided which should be terminated into floor level drain
Operating environment conditions +18 to +23°C (+64 to 73°F), 85% max RH (non condensing) ambient