Optional testing facilities

All Ascott test chambers are supplied complete and ready to run. The following optional accessories may not therefore be necessary, but some may be considered desirable. Use the menu above to select other chamber accessory sections.

F = factory fitted only  A = available separately

Optional accessory

Reference   

Description

F/A

 

Kit for Renault D17 2028(ECC-1)compliance

ACC01/†

A convenient kit of all necessary accessories (at a specially discounted price) to equip a CC1000ip chamber for compliance with ECC-1. Two versions of this kit are offered, featuring two choices of climate control unit. See graph on page 5 for differences in range of operation.

† Specify as: ACC01/1 to include the ACC80/1000 & ACC90/1000 options ACC01/2 to include the ACC112/1000 & ACC112/INTERFACE/1000 options.

Note: Only suitable for use with CC1000ip chambers.

F

 

Air Conditioner Interface

Air Conditioner Interface

ACC29/INTERFACE/****

Pre-equips a CCT chamber with everything needed to connect it to an ACC29 air conditioning unit (available separately) The fitting of this interface enables the air conditioning unit to be procured at the same time as the chamber, or later if required.

**** Specify chamber size in Ltrs.

Note: not suitable for use with option ACC46.

F

 

Air Conditioning

Air Conditioning ACC29TEMP

ACC29/TEMP - refrigeration control only

A separate and freestanding air conditioning unit to provide a refrigerated atmosphere inside the chamber from ambient to below freezing. See graph on the CCT Specifications page for range of operation. Two types are available:

ACC29/TEMP/****/-20C for refrigeration to -20°C/-4°F
ACC29/TEMP/****/-40C for refrigeration to -40°C/-40°F

**** Specify chamber size in Ltrs.

Note: all versions of ACC29 require the chamber to be pre-equipped with option: ACC29/INTERFACE.

A

 

Air Conditioning

Air Conditioning ACC29HUMIDITY

ACC29/HUMIDITY - Refrigeration & humidity control

A separate and freestanding air conditioning unit to provide refrigeration & humidity control inside the chamber. Refrigeration control is from ambient to below freezing. Humidity control is from ambient to -+10°C/50°F above freezing. See graph on the CCT Specifications page for range of operation. Two types are available:

ACC29/HUMIDITY/****/-20C for refrigeration to -20°C/-4°F
ACC29/HUMIDITY/****/-40C for refrigeration to -40°C/-40°F

**** Specify chamber size in Ltrs.

Note: all versions of ACC29 require the chamber to be pre-equipped with option: ACC29/INTERFACE.

A

 

Midi dehumidification unit

>Midi dehumidification unit ACC112

ACC112/****

A mid-size, air conditioning unit, to enable controlled 'ambient' climates to be created within a CCT chamber, independent of the temperature and humidity of the room in which it is located. See graph on the CCT Specifications page for range of operation.

**** Specify chamber size in Ltrs.

Note: all versions of ACC112 require the chamber to be pre-equipped with option ACC112/INTERFACE

A

 

Interface for ACC112

ACC112/INTERFACE/****

Pre-equips a CCT chamber with everything needed to connect it to an ACC112 midi dehumidification unit (available separately) The fitting of this interface enables the midi dehumidification unit to be procured at the same time as the chamber, or later if required. Note: not suitable for use with option ACC46.

**** Specify chamber size in Ltrs.

F

 

Salt spray (vertically down)

Salt spray vertically down

ACC30/****

High level, multiple spray nozzles which spray salt water directly down onto the samples under test. Spray time and duration are both user programmable. A separate holding tank holds salt water at ambient temperature. Required by SAEJ2334 and some GM tests.

**** Specify chamber size in Ltrs.

F

 

Water fog humidity

ACC32/****

Provides high humidity conditions (95 -100% RH) by spraying water as a fog. Includes an additional reservoir for water, fog atomizer(s) and associated pumping equipment.

**** Specify chamber size in Ltrs.

F

 

Liquid Immersion Interface

ACC34/INTERFACE/****

Pre-equips a CCT chamber with everything needed to connect it to an ACC34 liquid immersion facility (available separately) The fitting of this interface enables the liquid immersion facility to be procured at the same time as the chamber, or later if required.

Note: not suitable for use with option ACC46.

**** Specify chamber size in Ltrs.

F

 

Liquid Immersion

Liquid Immersion

ACC34/****

Under programmed control, heated immersion liquid (usually salt water heated to a user adjustable temperature up to +50°C/+122°F) is automatically pumped from the holding tank into the chamber, immersing the test samples. The liquid is automatically returned to the holding tank at the end of the immersion period.

Note: all versions of ACC34 require the chamber to be pre-equipped with option: ACC32/INTERFACE.

**** Specify chamber size in Ltrs.

A

 

Wall wash

ACC42/****

Comprises of a water spray rig to automatically wash the internal walls of the chamber with water. Both wash time and duration are user programmable. Requires the chamber to be connected to a continuous pressurized water supply of suitable quality and temperature.

**** Specify chamber size in Ltrs.

F

SO2 Gas Dosing

SO2 Gas Dosing

ACC46/****

Designed to meet the requirements of ASTM G85 annex A4, this optional accessory comprises of a chamber mounted dispersion tube, through which SO2 gas is introduced, at a user adjustable rate and for a programmable duration.

**** Specify chamber size in Ltrs

Notes:
1. The provision of the SO2 gas cylinder and connector are the users responsibility and are not included as part of this option.
2. The ACC46 is not suitable for use with options: ACC10, ACC29/INTERFACE, ACC34/INTERFACE, ACC92 and ACC112/INTERFACE.

A

 

Interface for ACC90

ACC80*

Pre-equips a CCT chamber with everything needed to connect it to an ACC90 dehumidifier (available separately) The fitting of this interface enables the dehumidifier to be procured at the same time as the chamber, or later if required.

* Specify as: ACC80/450/1000 for 450 or 1000 Ltr chambers & ACC80/2000 for 2000 Ltr chambers

F

 

Multi-solution salt spray

ACC86/****

Enables up to three different salt spray climates to be created which can be individually programmed to occur within any test program. Additional salt solution reservoirs, atomizers etc, are included.

**** Specify chamber size in Ltrs

F

 

Dehumidifier

ACC90

To deliver dehumidified air to CCT chambers where humidity control at, or just below ambient conditions, is required. See graph for range of operation.

Note: ACC90 requires the chamber to be pre-equipped with option: ACC80/INTERFACE (available separately).

**** Specify chamber size in Ltrs.

F

 
Got to the Ascott On-line Shop
Got to the Ascott Corro-Salt website
Got to the Ascott On-line Shop