Related Tests
Other standards which are referenced by ASTM G85, and which may be used to complement the information included in this site, include:
ASTM B117 (click here for details)
Practice for Operating Salt Spray (Fog) Testing
ASTM D609
Practice for Preparation of Cold-Rolled Steel Panels for Testing Paint, Varnish, Conversion Coatings, and Related Coating Products
ASTM D1141 (click here for details)
Specification for Substitute Ocean Water
ASTM D1193 (click here for details)
Specification for Reagent Water
ASTM D1654
Test Method for Evaluation of Painted or Coated Specimens Subjected to Corrosive Environments
ASTM E70
Test Method for pH of Aqueous Solutions with the Glass Electrode
A tabular summary of all the major salt spray and cyclic corrosion tests (click here) is available.