ASTM B117



Related Tests

Other standards which are referenced by ASTM B117, and which may be used to complement the information included in this site, include:

ASTM B368 (click here for details)
Copper Accelerated Acetic Acid Salt Spray (Fog) Testing.

ASTM D1193 (click here for details)
Specification for Reagent Water.

ASTM G85 - Modified Salt Spray (Fog) Testing.
This test standard comprises of 5 climate modifications to the basic salt spray test:

ASTM G85 annex A1 (click here for details)
Acetic acid salt spray test, continuous.

ASTM G85 annex A2 (click here for details)
Cyclic acidified salt spray test.

ASTM G85 annex A3 (click here for details)
Seawater acidified test, cyclic.

ASTM G85 annex A4 (click here for details)
Sulphur dioxide (SO2 ) salt spray test, cyclic.

ASTM G85 annex A5 (click here for details)
Dilute electrolyte cyclic fog /dry test.

ASTM D609
Practice for Preparation of Cold Rolled Steel Test Panels for Testing Paint, Varnish, Conversion Coatings and Related Coating Products.

ASTM D1654
Test Method for Evaluation of Painted or Coated Specimens Subject to Corrosive Environments.

ASTM D1193 (click here for details)
Specification for Reagent Water.

ASTM E70
Test Method for pH of Aqueous Solutions with the Glass Electrode.

ASTM E691
Practice for Conducting an Interlaboratory Study to Determine the Precision of a Test Method.


A tabular summary of all the major salt spray and cyclic corrosion tests (click here) is available.

 

 